COATING TYPE: AQUA-EPOXY WATERBORNE DISPERSION

AQUA-EPOXY: Waterborne dispersion two-component epoxy-copolymer with dehydrated V.O.C. range of 1.4-2.3, for use as a primer-topcoat or direct-to-metal paint. Has an initial gloss of 85-90% (60 deg. head) with good depth of image. Possesses excellent gloss retention superior to standard solvent borne epoxies and has good chemical and corrosion resistance.

MIXING RATIO: 4:1
POT LIFE: 8-10 HRS
PUMP PRESSURE: 1800-2100 psi
TIP SIZES: 6, 19; 6, 21’S
FILTERS: 60 MESH
MIN STEEL TEMP: 50 deg F
MIN APPLICATION TEMP: 50 deg F
REQUIRED WET MILS: 10-12
SPRAY TECHNIQUE: SINGLE CROSS COAT,
30% OVERLAP
DRY TO TOUCH: 6-8 HRS
MIN RECOAT TIME: 6-8 HRS
EQUIPMENT REQUIREMENTS: AIRLESS
V.O.C.: 1.4-2.3 DEHYDRATED
SUBSTRATE PREP: SSPC-SP-6
D.O.T.: NON-FLAMMABLE
SWEAT IN TIME: 15 MIN
THINNING: SEE **
SOLVENT TYPE: WATER
REDUCTION: SEE ***
VISCOSITY: THIXOTROPIC
MAX STEEL TEMP: 85 deg F
MAX APPLICATION TEMP: 85F
REQUIRED DRY MILS: 3-3.5
THROUGH DRY: 24 HRS
MAX RECOAT TIME: WILL NOT LIFT
SOLIDS BY VOLUME: 38-42%
FREEZE THAW: NONE